Spherical Aluminum Alloy Powder
ACME uses PREP method, which is using metal or alloy as the consumable electrode, and under the centrifugal force to produce spherical metal powder. This method avoid the slug and contact with refractory material, eliminate the non-metal impurities, and produce high purity spherical powder.
- Kev Nta
- Lwm yam xaiv xaiv configuration
Spherical Aluminum Alloy Powder
qib | Tshuaj Muaj pes tsawg leeg | Cov Qauv Khoom | Particle Loj Distribution | ||
Main Element | Impurity Element | Lub teb chaws tus qauv | Tebchaws USA cov qauv | ||
AlSi 10Mg (ZL104) | Si:10-11 Mg:0.4-0.45 Fe:0.14-0.55 Cu:<0.05 Mn:<0.01-0.45 Al:Bal | Ni:<0.01-0.05 Zn:<0.01-0.1 Pb:<0.01-0.05 Sn:<0.01-0.05 Ti:<0.01-0.15 O :<0.05 | GB / T 1173-2013 | 15-45μm 15-53μm 53-120μm 53-150μm | |
AlSi 12 (ZL102) | Fe:≤0.25 Mn:≤0.1 Si:11.00-13.00 Zn:≤0.2 Al: Bal | Cu:≤0.3 Mg:≤0.1 Pb:≤0.02 Sn:≤0.02 O :<0.05 | GB / T 1173-2013 | 15-45μm 15-53μm 53-120μm 53-150μm | |
AlSi 7Mg (ZL101) | Si:6.5-7.5 Mg:0.25-0.45 Al: Bal | O:<0.05 | GB / T 1173-2013 | 15-45μm 15-53μm 53-120μm 53-150μm | |
7A04 | Cu:1.4-2.0 Mn:0.2-0.6 Mg:1.8-2.8 Cr:0.1-0.25 Zn:5.0-7.0 Al: Bal | Si:0.5 Fe:0.5 Ti:0.1 O :<0.05 Res Each:0.05 Res Total:0.1 | GB / T 3190-2008 | 15-45μm 15-53μm 53-120μm 53-150μm | |
2A12 | Cu:3.8-4.9 Mn:0.3-0.9 Mg:1.2-1.8 Al:Bal | Si:0.5 Fe:0.5 Ni:0.1 Zn:0.3 Ti:0.15 O :<0.05 Res Each:0.05 Res Total:0.1 | GB / T 3190-2008 | 15-45μm 15-53μm 53-120μm 53-150μm | |
2A14 | Cu:3.9-4.8 Mn:0.4-1.0 Mg:0.4-0.8 Si:0.6-1.2 Al: Bal | Fe:0.7 Ni:0.1 Zn:0.3 Ti:0.15 O :<0.05 Res Each:0.05 Res Total:0.1 | GB / T 3190-2008 | 15-45μm 15-53μm 53-120μm 53-150μm |